General Applications
- Heat-resistant molds for silicone or urethane
- Thermal test fixtures or functional prototypes
- Components near heat sources (e.g., lamps, motors)
- Functional parts for warm environments
- Industrial jigs or high-temp tools
Advantages
- High thermal resistance
- Short-term stability under heating
- Suitable for molding
Disadvantages
- Brittle and rigid
- Typically dull/rough surface finish
Colors
Not available
Specification
| Property | Value |
|---|---|
| Technology | SLA |
| Shrinking Rate | Medium (~5 - 7%) |
Physical Properties
| Property | Testing Method | Typical Value |
|---|---|---|
| Density | GB/T 4472 | 1.09 - 1.10 g/cm³ |
| Viscosity | GB/T 2235 | 650 mPas |
| Light Transmission | N/A | N/A |
| Flame Retardancy | N/A | N/A |
Chemical Resistivity
| Effect | Value |
|---|---|
| Effect of weak acid | N/A |
| Effect of strong acid | N/A |
| Effect of weak alkaline | N/A |
| Effect of strong alkaline | N/A |
| Effect of oil and grease | N/A |
Thermal Properties
| Property | Testing Method | Typical Value |
|---|---|---|
| Heat Deflection Temp | GB/T 1634 | > 280°C at 0.45 MPa |
Mechanical Properties
| Property | Testing Method | Typical Value |
|---|---|---|
| Tensile Strength | ASTM D638 | 53.3 MPa |
| Flexural Strength | ASTM D790 | 92.7 MPa |
| Elongation at Break | ASTM D638 | 6.4 % |
| Notched Izod (Machined), 23°C | ASTM D256 | 17 J/m |
| Shore Hardness | ASTM D2240 | 83 - 84D |
Last updated: 6/15/2025